PDF
…36±3%, ind
Resin Content
ASTM D 3529
Every roll(2)
36±2%, avg
ASTM D 3776 or
370±16 gsm, ind
Fiber Areal Weight
SACMA SRM
Every roll(2)
370±14 gsm, avg
23R-94
First and last rolls
Volatile Content
ASTM D 3530
1.5% max, avg
of every batch(2)
First and last rolls
Flow
ASTM D 3531
15.4 to 19.4%, avg
of every batch(2)
19.97 to 27.67
Gel Time
ASTM D 3532…
https://www.wichita.edu/industry_and_defense/NIAR/Research/cytec-5250-5/T650-6k-5HS-1.pdf